UJI BENDING DAN APLIKASI WPS PADA PLAT KAPAL TANKER DENGAN GAP 2 MM DI PT. DAYA RADAR UTAMA LAMPUNG
DOI:
https://doi.org/10.37338/inovator.v3i1.125Keywords:
Pengelasan, WPS, GAP, Uji BendingAbstract
The ship production process is largely a welding work. About one-third of the total number of jobs in the construction stage is regulated Welding Procedure Specification (WPS) which is regulates welding rules such as class material, electrodes, how to weld the bevel shape long distance bevel (gap) and slope angle. Based on the WPS used of construction HN 309 Tanker Ship the length of the bevel distance (gap) in welding SMAW is 2,63 mm. Bending tests are performed to regulate strength of materials due to loading without causing deformation. This research study aims to determine the bending strength (quality) of the welders is 1 mm plate with variants of are 100 A 120 A and 140 A. The welding method ASTM A36 plate which is do bending test to using MTS landmark ASTM E 190-2003. The flexural strength of bending test from the three specimens based on current variation is the value of current strength 140 A is best compared to the current strength of 120 A and 100 A, the value of 140 current strength is 1.76107649 kN /mm2, current value of 120 A is 1,50230752 KN/mm2 and 100 A current strength of 1,44976202 kN /mm2 with a linear regression value is 0,872. So that the 11 mm plate welding procedure with a 2 mm gap can be used in the ship building production process.
References
Sulaiman, Eko Julainto S. 2015. Perlakuan Nilai Kekerasan Plat Baja Kapal Dengan Perlakuan Bending Line Heating. Jurnal TEKNIS, Volume 10, Nomor 2, 76-80
Waseso Purbo, Edi Riyanto. 2018. Analisa Pengaruh Kuat Arus listrik Terhadap Kekuatan Tarik dan Tekuk pada Joint Alumunium Alloy 5083. Jurnal Teknik Perkapalan Um Surabaya Volume 1 Nomor 1. 46
Suprijanto Djoko. 2013. Pengaruh Bentuk Kampuh Terhadap Kekuatan Bending Las Sudut SMAW posisi Mendatar Pada Baja Karbon Rendah. Jurnal Teknik Mesin STTNAS Yogyakarta. M 91.
Syaripuddin, Imam Basori, dan Yunata Mandala Putra. 2014. Pengaruh Jenis Kampuh Las Terhadap Kekuatan Tarik Baja Paduan Rendah (ASTM A36) Menggunakan Las SMAW. Jurnal Konversi Energi dan Manufaktur UNJ, Edisi terbit II, 95.
Sunaryo, Heri. 2008. Teknik Pengeasan Kapal Jilid I. Direktorat Pembinaan Sekolah Kejuruan:Jakarta.
Ahmad Naufal, Sarjito Jokosisworo, Samuel. 2016. Pengaruh Kuat Arus Listrik Dan Sudut Kampuh V Terhadap Kekuatan Tarik Dan Tekuk Aluminium 5083 Pengelasan GTAW. Jurnal Teknik Perkapalan Universitas Diponegoro Vol 2. 256.
Wibowo Ari Tyas, Wahyu Purwo Raharjo, dan Bambang Kusharjanta. 2014. Perancangan Dan Analisa Kekuatan Kontruksi Mesin Tekuk Plat Hidrolik. Jurrnal Mekanika Volume 12 Nomor 2. 63.
M. Yogi Nasrul L, Heru Suryanto, Abdul Qolik. 2016. Pengaruh Variasi Arus Las SMAW Terhadap Kekerasan Dan Kekuatan Tarik Sambungan Dissimilar Stainless Steel 304 Dan St 37. Jurnal Teknik Mesin Universitas Negeri Malang. Edisi Terbit I. 10.
Badarudin. 2019. MTSL Flexural Test Badaruddin. Fakultas Teknik Mesin Universitas Lampung: Lampung.
Downloads
Published
Issue
Section
License
Copyright (c) 2020 Yulli Indriyanti, Kurniawati Oktarina, Suzi Heti Kurnia

This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.